چکیده
|
Effect of tool rotation rate and traverse speed on strain hardening behavior of friction stir welded
(FSWed) copper joints were investigated using hardening capacity and strain hardening exponent concepts.
Kocks–Mecking type plots were used to show different stages of strain hardening. FSWed samples
reveals higher hardening capacity and lower strain hardening exponent relative to base metal. With
increasing rotation rate and/or decreasing traverse speed, FSWed samples show higher hardening capacity
and lower strain hardening exponent. The strain hardening behavior was discussed by dislocation
density and grain size variation during FSW. In addition, the microstructure and mechanical properties
of the samples were investigated in detail. Four different zones were observed in microstructure of
FSWed joints. The joints showed finer grain structure and weaker mechanical properties relative to base
metal due to dynamic recrystallization and lower dislocation density.
|